Review of Previous Water Research Foundation Projects on Galvanic Corrosion
Associated Project
Project 4349: Galvanic Corrosion Following Partial Lead Service Line ReplacementDescription
- Effect of Changing Disinfectants on Distribution System Lead and Copper Release, Part 2 (project 3107) concluded that galvanic corrosion affects lead release but that the galvanic effects are transient and short-lived.
- Contribution of Galvanic Corrosion to Lead (Pb) in Water after Partial Lead Service Line Replacements (project 4088b) reported that galvanic corrosion can be a substantial and long-term source of lead release.
Consequently, the scope of this review is primarily focused on these two reports, but also includes other relevant work conducted on the topic.
- Effect of Changing Disinfectants on Distribution System Lead and Copper Release, Part 2 (project 3107) concluded that galvanic corrosion affects lead release but that the galvanic effects are transient and short-lived.
- Contribution of Galvanic Corrosion to Lead (Pb) in Water after Partial Lead Service Line Replacements (project 4088b) reported that galvanic corrosion can be a substantial and long-term source of lead release.
Consequently, the scope of this review is primarily focused on these two reports, but also includes other relevant work conducted on the topic.